STANDARDS - TITANIUM ANODES | |
MMO Coating by Thermal decomposition | |
Composition Basis : RuC13, IrC13, TiC14, TaC15 | |
Density : Genarally Between 6 - 12 grams per cubic Cm.Variousdepending upon the appalication. | |
Cable connection : As per International standard. | |
Anode cable resistence : 0.001 ohms(Max) | |
Hellum leak test (Sniff) : 200 KPa gage ( 2 atomspheres) |
Electrolyte | Max.C.D | Anode Life |
Carbonaceous Backfill | 50 A/Sq M | 20 Years |
Calcined petroleum coke | 100 A/Sq M | 20 Years |
Fresh Water | 100 A/Sq M | 20 Years |
Brackish Water | 300 A/Sq M | 20 Years |
Sea Water | 600 A/Sq M | 20 Years |